When working with polyurethane, it is important not only to choose the right material. The entire technological process affects the casting result – from storing the components to preparing the mold and the moment of demolding.

Sometimes the material is selected correctly, but the finished part still has bubbles, porosity, an uneven surface or does not gain the required hardness.

In this article, we will consider the 5 most common mistakes that we have to deal with:

1. The components are at the wrong temperature

The temperature directly affects the viscosity of the components, their mixing and the speed of reaction.

If the material is too cold, it can become more viscous, mix worse and fill the mold more slowly. If the temperature is too high, the reaction can proceed faster, reducing the working time.

Therefore, before starting work, it is worth checking the temperature of the components and following the recommendations for a specific system.

2. Moisture gets into the material

Moisture can be a serious problem for polyurethane systems.

Its entry into the components or the mold can cause bubbles, porosity and other defects in the finished part.

This is especially important after opening the container. The components must be stored according to the manufacturer’s recommendations and do not leave the containers open.

It is also important to pay attention to the mold – it must be clean and dry before pouring.

3. Components are not mixed correctly

Even the correct ratio of components will not help if they are not mixed sufficiently or unevenly.

When mixing by hand, it is necessary to ensure the homogeneity of the mixture, while trying not to entrap excess air.

When mixing by machine, it is important to monitor the operation of the dosing system and mixing unit.

Uneven mixing can lead to differences in hardness or degree of hardening in different parts of the part.

4. Violation of the component ratio

Each polyurethane system has a recommended component ratio.

Deviation from it can change not only the curing time, but also the final properties of the material – hardness, strength and elasticity.

Therefore, dosing “approximately” is not the best option. For a stable result, the components must be dosed accurately.

5. The mold is improperly prepared

The mold is in direct contact with the future part, so its condition is very important.

Before pouring, you need to make sure that the mold is clean, dry and properly prepared. If necessary, use an appropriate release agent, which is applied with a very thin layer

An incorrectly applied or inappropriate release agent can affect the surface of the part and make demolding difficult.

And the remains of the previous material, dust or moisture can cause surface defects.

You should also monitor the temperature of the mold, which should be the same as the reaction temperature of the material.

This is not a universal diagnosis – the same problem can have several causes. But such a simple checklist will help you start the search.

Correctly selected polyurethane, compliance with the temperature regime, accurate dosage, high-quality mixing, dry form and the right separator – all these are parts of one technological process. Therefore, before replacing the material, it is worth checking the technology itself.

And if you cannot determine the cause yourself – contact OSV Polymer. We will help you understand the possible causes of defects and select a polyurethane system according to the specific task.